Blog, Manufacturing

How to Evaluate Pull-Out Force in Crimp Terminals: Testing Methods and Quality Standards

pull-out test

Introduction

A crimp terminal must provide more than a reliable electrical connection. It must also maintain sufficient mechanical strength to prevent the wire from loosening, slipping out, or separating from the terminal during installation and operation.

Table of Contents

Pull-out force is one of the most important mechanical indicators used to evaluate crimping quality. It measures how much tensile force a crimped connection can withstand before the conductor pulls out, breaks, or the connection otherwise fails.

For manufacturers of electrical terminals, wire harnesses, and electrical assemblies, pull-out force testing helps verify crimping processes, identify potential production defects, and maintain consistent product quality.

In this guide, we explain how to evaluate pull-out force in crimp terminals, the testing methods involved, the factors affecting test results, common failure modes, and how manufacturers can improve crimp connection reliability.

1. What Is Pull-Out Force in a Crimp Terminal?

Pull-out force is the tensile force required to separate a conductor from a crimped terminal. It evaluates the mechanical retention strength between the terminal barrel and the wire conductor.

During crimping, the terminal barrel is compressed around the conductor, creating a mechanical connection through controlled deformation. A properly designed and manufactured crimp should hold the conductor securely without damaging its strands or compromising electrical performance.

Pull-out force is typically measured in Newtons (N).

pull-out test 2

Pull-Out Force vs. Tensile Strength

Although these terms are related, they describe different properties.

  • Pull-out force: The force required to separate the wire from the crimped terminal.
  • Wire tensile strength: The force a conductor or wire can withstand before breaking under tension.
  • Crimp connection strength: The mechanical integrity of the complete crimped connection, including the conductor and terminal barrel.

During a pull-out test, the conductor may slide out of the terminal, break near the crimp, or the terminal barrel may deform or fail. The observed failure mode is important when interpreting the test result.

What Does Pull-Out Force Testing Evaluate?

A pull-out force test helps evaluate:

  • Mechanical retention between the conductor and terminal
  • Crimp compression and conductor deformation
  • Resistance to wire slippage
  • Compatibility between the terminal and wire size
  • Consistency of the crimping process

It is an important quality control method, particularly for applications involving vibration, mechanical movement, or demanding installation conditions.

2. Why Pull-Out Force Testing Is Important

Preventing Wire Separation

A weak crimp may allow the wire to loosen or detach from the terminal during handling, installation, or operation.

In automotive wiring harnesses, industrial electrical equipment, and power distribution assemblies, mechanical separation can interrupt circuits, create intermittent connections, or lead to equipment failure.

Pull-out force testing helps identify insufficient conductor retention before terminals are used in finished products.

Supporting Electrical Connection Reliability

Mechanical and electrical performance are closely related in crimped connections.

An improperly crimped conductor may have inadequate contact between the wire strands and terminal barrel. This can contribute to unstable electrical contact, increased contact resistance, and localized heating under current load.

However, pull-out force alone cannot confirm electrical performance. A crimp connection should also be evaluated using appropriate electrical tests, such as contact resistance measurement, where required.

Verifying Manufacturing Quality

Pull-out force testing is commonly used during:

  • New terminal development
  • Crimp tooling validation
  • First-article inspection
  • Production process verification
  • Customer quality audits
  • Corrective action investigations

By comparing test results with established acceptance criteria, manufacturers can identify process deviations and improve production consistency.

3. How to Measure Pull-Out Force in Crimp Terminals

Pull-out force is generally measured using a tensile testing machine or universal testing machine equipped with suitable fixtures.

Equipment Required

A typical testing setup includes:

  • Universal tensile testing machine
  • Appropriate load cell
  • Terminal holding fixture
  • Wire gripping fixture
  • Force measurement and data recording system

The load cell should have a suitable measurement range for the expected pull-out force. Using an excessively large load cell may reduce measurement resolution, while an undersized load cell may exceed its capacity.

The fixtures should securely hold the terminal and conductor without introducing additional damage or slippage.

Step-by-Step Pull-Out Force Test Procedure

Step 1: Prepare the test specimen

Select the terminal and wire according to the specified product requirements. Confirm the conductor cross-section, wire construction, terminal model, and stripping length.

Crimp the wire using the specified tooling and production parameters.

Step 2: Mount the specimen

Secure the terminal in the testing fixture and clamp the wire in the tensile testing machine.

The gripping method should prevent wire slippage without damaging the conductor outside the crimped area.

Step 3: Align the pulling direction

The wire should be pulled along its axis to minimize bending, twisting, or side loading.

Misalignment can introduce additional forces and affect the accuracy and repeatability of the test.

Step 4: Apply tensile force

The testing machine applies a controlled tensile load to the wire.

The pulling speed should follow the applicable testing standard or customer specification. For standardized tests, it is important not to change the test speed between specimens when comparing results.

Step 5: Record the maximum force

Record the peak tensile force reached before the connection fails, the conductor breaks, or the specified test endpoint is reached.

The measured value is generally reported in Newtons (N).

Step 6: Inspect the failure mode

After testing, examine the terminal and conductor to determine how the connection failed.

The failure mode provides valuable information for diagnosing crimping problems and improving the manufacturing process.

Important Test Conditions

For reliable and repeatable results, the following conditions should be controlled:

  • Pulling speed
  • Specimen alignment
  • Terminal and wire gripping method
  • Wire stripping length
  • Crimping parameters
  • Test equipment calibration
  • Sample preparation
  • Test environment, where specified

Test conditions should be documented to ensure that results can be compared accurately across production batches.

4. Standards for Crimp Terminal Pull-Out Force Testing

Industry standards provide test methods and reference requirements for evaluating crimped connections. However, the applicable standard depends on the terminal design, conductor type, application, and customer requirements.

IEC 60352-2

IEC 60352-2 covers solderless crimped connections, including general requirements, test methods, and practical guidance for applicable crimp connections.

Its mechanical testing section specifies pull-out force testing in accordance with Test 16d of IEC 60512.

The standard also provides reference minimum pull-out force values for specified conductor cross-sections. These values should be applied only where the connection falls within the standard’s applicable scope.

IEC 60512-16-4, Test 16d

IEC 60512-16-4 describes a tensile test method for evaluating the mechanical strength of crimped connections.

The test applies tensile force axially to the conductor until the wire is pulled out or breaks. The test speed and conditions must follow the applicable requirements.

For standardized testing, the test method should be followed consistently rather than using an arbitrary pulling speed or fixture arrangement.

Customer-Specific Requirements

In automotive, industrial, and electrical equipment applications, customers may establish their own pull-out force requirements based on:

  • Terminal design
  • Wire specification
  • Operating environment
  • Vibration requirements
  • Assembly conditions
  • Product reliability expectations

A manufacturer should always confirm the applicable specification before determining whether a test result is acceptable.

5. Pull-Out Force Reference Values by Wire Size

Conductor cross-sectional area is one of the main factors influencing the required pull-out force.

Larger conductors generally require higher mechanical retention forces. However, the relationship is not necessarily linear because terminal geometry, material properties, and crimp design also affect the result.

The following table presents selected reference values from IEC 60352-2 for applicable crimped connections.

Conductor Cross-SectionApprox. AWGReference Pull-Out Force
0.05 mm²306 N
0.08 mm²2811 N
0.12 mm²2615 N
0.14 mm²—18 N
0.22 mm²2428 N
0.25 mm²—32 N
0.32 mm²2240 N
0.50 mm²2060 N
0.75 mm²—85 N
0.82 mm²1890 N
1.00 mm²—108 N
1.30 mm²16135 N
1.50 mm²—150 N
2.10 mm²14200 N
2.50 mm²—230 N
3.30 mm²12275 N
4.00 mm²—310 N
5.30 mm²10355 N
6.00 mm²—360 N
8.40 mm²8370 N
10.00 mm²—380 N

Note: These are reference values from IEC 60352-2 for applicable crimped connections. They are not universal acceptance criteria for every terminal design. Verify the relevant standard edition, product specification, and customer requirements before using them for qualification or production inspection.

How to Interpret Pull-Out Force Results

A test result should be evaluated against the applicable minimum requirement.

  • Below the specified minimum: The crimp connection may have insufficient mechanical retention and requires investigation.
  • Meeting the specified requirement: The connection meets the pull-out force criterion, but other quality characteristics must still be evaluated.
  • Significantly above the requirement: The result may indicate strong mechanical retention, but it does not automatically prove that the crimp is optimized.

Excessive crimp compression can damage conductor strands, reduce the effective conductor cross-section, or affect electrical performance. A good crimp is one that meets mechanical and electrical requirements while maintaining consistent process quality.

6. Key Factors Affecting Pull-Out Force

Crimp Height and Compression

Crimp height is one of the most important parameters influencing mechanical retention.

If the terminal is under-crimped, the conductor may not be sufficiently compressed within the barrel, allowing the wire to slip out under tensile loading.

If the terminal is over-crimped, conductor strands may become damaged or excessively deformed. This can reduce the effective conductor cross-section and potentially compromise long-term reliability.

Maintaining the correct crimp height is essential for achieving consistent pull-out force.

Wire Size and Conductor Structure

Pull-out force is influenced by the conductor’s cross-sectional area, strand count, strand diameter, and material.

Different wire constructions may behave differently during crimping, even when they have the same nominal cross-sectional area.

The terminal barrel must be appropriately designed for the conductor size and construction to achieve adequate mechanical retention.

Terminal Material and Barrel Design

Terminal materials such as copper, brass, and phosphor bronze have different mechanical properties.

Material thickness, hardness, barrel width, barrel depth, and crimp geometry all influence how the terminal deforms around the conductor.

Open-barrel and closed-barrel terminal designs may also require different crimping parameters and validation methods.

Crimping Tool and Die Accuracy

Crimping tooling directly affects the shape and compression of the finished connection.

Worn dies, incorrect applicator settings, poor alignment, or inaccurate tooling dimensions can lead to inconsistent crimp height and reduced pull-out force.

Precision tooling and regular maintenance help maintain stable crimping quality during mass production.

Crimping Process Consistency

Even when terminal and wire specifications are correct, process variation can affect pull-out force.

Important factors include:

  • Crimping force
  • Crimp height adjustment
  • Wire positioning
  • Strip length
  • Machine condition
  • Production speed
  • Tool wear

A stable manufacturing process is essential for achieving repeatable test results across production batches.

7. Common Pull-Out Test Failure Modes

Understanding how a crimp connection fails is just as important as recording the maximum force.

pull-out test 3

Wire Pulls Out of the Terminal

This failure occurs when the conductor separates from the terminal barrel before the required force is reached.

Possible causes include:

  • Insufficient crimp compression
  • Incorrect terminal-to-wire size matching
  • Improper crimping tooling
  • Poor conductor positioning
  • Incorrect strip length

The crimping process and terminal compatibility should be reviewed.

Conductor Breaks Near the Crimp

A conductor break near the crimped area may indicate that the wire has been weakened during crimping.

Possible causes include excessive compression, damaged strands, sharp terminal edges, or improper crimp geometry.

The test result should be interpreted alongside the failure location and conductor condition.

Terminal Barrel Deforms or Cracks

Terminal barrel deformation or cracking may result from excessive crimping force, unsuitable material properties, incorrect tooling, or a design issue.

The terminal material, thickness, hardness, and tooling configuration should be examined.

Inconsistent Test Results

Large variations between specimens may indicate unstable production conditions or inconsistent testing methods.

Potential causes include:

  • Inconsistent crimp height
  • Tool wear
  • Different wire positioning
  • Improper fixture alignment
  • Wire slippage during testing
  • Equipment calibration issues

Repeated testing and process analysis can help identify the source of variation.

8. How Manufacturers Improve Pull-Out Force Performance

Improving pull-out force requires more than increasing crimping pressure. The objective is to achieve reliable mechanical retention without damaging the conductor or terminal.

Optimize Crimping Parameters

Manufacturers should establish validated crimping parameters, including crimp height, tooling configuration, and process settings.

Regular inspection helps identify deviations before they affect large production batches.

Develop Accurate Terminal Tooling

Precision stamping dies and crimping applicators help maintain terminal geometry and dimensional consistency.

Tooling design, die accuracy, and maintenance directly influence the quality of the finished crimp.

Match Terminal Design to Wire Specifications

Terminal barrel dimensions should be compatible with the intended conductor size and construction.

A well-designed crimping structure provides sufficient conductor retention while avoiding excessive deformation.

Implement Routine Quality Testing

Pull-out force testing should be integrated into a structured quality control process.

Depending on the production requirements, testing may be performed during initial setup, tooling changes, process validation, routine production sampling, or corrective action investigations.

Combine Mechanical Testing With Other Inspections

Pull-out force should not be used as the sole indicator of crimp quality.

Inspection MethodPurpose
Pull-out force testEvaluates mechanical retention
Crimp height measurementVerifies crimp compression consistency
Crimp cross-section analysisExamines conductor deformation and strand distribution
Visual inspectionIdentifies visible crimp defects
Contact resistance testEvaluates electrical connection performance
Temperature-rise testEvaluates performance under electrical loading where required

A comprehensive inspection plan helps verify both mechanical and electrical reliability.

9. Pull-Out Force Testing for Different Types of Electrical Terminals

Different terminal structures require appropriate crimping processes and validation methods.

 

Ring Terminals

Ring terminals are widely used in grounding, power distribution, automotive wiring, and electrical equipment.

Pull-out force testing evaluates the mechanical retention of the conductor within the crimp barrel. Consistent crimping is important to prevent wire separation during installation or service.

Spade and Fork Terminals

Spade and fork terminals are commonly used in electrical connections where convenient installation and removal are required.

The wire crimp section must provide adequate conductor retention while maintaining the terminal’s intended connection geometry.

Terminals on Reel

Terminals on Reel are designed for automated wire processing and high-volume production.

Consistent terminal dimensions, strip alignment, and crimping performance are essential for maintaining production efficiency and repeatability.

Pull-out force testing can help verify the stability of the crimping process across production batches.

Automotive Crimp Terminals

Automotive terminals are often exposed to vibration, temperature changes, and demanding operating conditions.

Mechanical retention, conductor integrity, crimp consistency, and electrical performance must be evaluated according to the applicable automotive and customer-specific requirements.

Custom Stamped Metal Terminals

Custom terminals require validation based on their specific geometry, material, conductor size, and application.

During product development, pull-out force testing helps verify whether the terminal barrel design and crimping process can achieve the required mechanical performance.

10. Establishing a Pull-Out Force Quality Control Plan

A structured quality control plan helps manufacturers maintain repeatable results and traceable inspection records.

Define Testing Requirements

Each product should have clearly defined testing requirements, including:

  • Terminal part number
  • Wire specification
  • Conductor cross-section
  • Crimping tooling
  • Required minimum pull-out force
  • Applicable test method
  • Sample size
  • Inspection frequency

Establish Sampling Frequency

A practical quality control framework may include:

Production StageRecommended Inspection
Initial production setupFirst-article pull-out testing
Tool or applicator changeVerification testing
Wire or terminal material changeValidation testing
Routine productionPeriodic sampling
Abnormal crimping conditionAdditional testing

The actual inspection frequency should be determined by the quality control plan, customer requirements, risk assessment, and production history.

Maintain Traceable Test Records

A pull-out force test report should record:

  • Test date
  • Terminal part number
  • Wire specification
  • Crimping machine and tooling
  • Crimp height
  • Test speed
  • Individual test results
  • Average and minimum measured force
  • Failure mode
  • Pass/fail status
  • Corrective action, if applicable

Monitor Process Consistency

Statistical analysis can help identify variation in pull-out force results.

Manufacturers may track average force, minimum and maximum values, standard deviation, and production trends.

Where sufficient data and appropriate process assumptions are available, statistical process control and process capability analysis can provide additional insight into manufacturing stability.

11. How to Evaluate Pull-Out Force When Sourcing Crimp Terminals

For buyers sourcing electrical terminals, pull-out force testing is an important part of supplier quality evaluation.

Request Test Reports

Ask the terminal manufacturer to provide relevant test data, including:

  • Pull-out force test reports
  • Applicable testing standards
  • Wire size and conductor specification
  • Testing conditions
  • Sample quantity
  • Test results
  • Failure modes

A test report should clearly identify the terminal and wire combination tested.

Verify That the Test Matches Your Application

Test results are meaningful only when the test conditions are relevant to the intended application.

Confirm that the tested terminal model, conductor size, wire construction, and crimping tooling match your requirements.

If the terminal will be used with a different wire or crimping process, additional validation may be necessary.

Evaluate Consistency, Not Just One Result

A single high pull-out force result does not necessarily demonstrate stable production quality.

Buyers should evaluate the manufacturer’s ability to maintain consistent crimping parameters, control tooling, conduct routine inspections, and provide traceable quality records.

Consider Manufacturing Capability

Reliable crimp terminals depend on accurate terminal dimensions, stable material properties, precision tooling, and controlled manufacturing processes.

When evaluating a supplier, consider its terminal stamping capability, tooling development, dimensional inspection, production process control, and ability to support custom terminal requirements.

Conclusion

Pull-out force is a key mechanical indicator for evaluating the quality and reliability of crimp terminals. It helps verify whether a crimped connection can withstand the required tensile load without conductor separation or unacceptable failure.

Reliable testing requires properly prepared specimens, suitable testing equipment, controlled pulling conditions, and clearly defined acceptance criteria.

However, pull-out force should not be evaluated in isolation. Crimp height, conductor condition, terminal geometry, contact resistance, and manufacturing consistency all contribute to the overall performance of a crimped connection.

For terminal manufacturers, a systematic testing and quality control process is essential for maintaining repeatable performance. For buyers, reviewing pull-out force data and the supplier’s testing capability can provide valuable insight into product quality and manufacturing reliability.

At Qianwei Precision, we manufacture standard and custom electrical terminals using precision stamping, tooling development, and controlled production processes. Whether you require ring terminals, spade terminals, terminals on reel, automotive terminals, or custom stamped metal terminals, our team can support your product requirements from design and tooling development to mass production.

Contact Qianwei Precision to discuss your terminal specifications, wire compatibility, and quality testing requirements.

Leave a Reply